كيف تمنع التآكل الجلفاني بين الألومنيوم والفولاذ المقاوم للصدأ؟
تم التحديث 16 أغسطس 2025
قراءة 5 دقائق

كيف تمنع التآكل الجلفاني بين الألومنيوم والفولاذ المقاوم للصدأ؟

Aluminum extrusion profile with powder coating to block galvanic contact
Powder-coated surface prevents metal-to-metal corrosion

When aluminum and stainless steel touch, corrosion can start silently. Left unchecked, it damages parts, weakens joints, and increases maintenance costs.

You can prevent galvanic corrosion between aluminum and stainless steel by isolating the metals with non-conductive materials, coatings, or proper design.

Mixing metals without planning leads to expensive repairs. But with the right steps, you can use both materials together safely. Let’s explore how.

What materials can isolate aluminum from stainless steel?

Many engineers overlook this step. But proper isolation is the most effective way to stop galvanic corrosion between aluminum and stainless steel.

You can isolate aluminum from stainless steel using plastic washers, rubber gaskets, nylon bushings, or painted surfaces that break the electrical path.

Anodized aluminum extrusion profile providing electrical insulation
Anodized barrier layer reduces galvanic reactions with stainless

Galvanic corrosion happens when two different metals touch in the presence of an electrolyte like water. One metal becomes the anode (corrodes), the other the cathode. Aluminum is the anode in this pair, meaning it will degrade faster.

Common Isolation Materials

Isolation Material Where to Use الملاحظات
Nylon washers Between bolts and aluminum surfaces Low-cost, easy to install
Rubber gaskets Between flanges, panels Also provides vibration damping
Plastic sleeves Around bolts or inside holes Fully insulates bolts from structure
الطلاء بالمساحيق On aluminum parts Avoids direct contact, needs inspection
Fiber or felt pads In temporary setups Not suitable for high-load areas

These materials block the electrical current. No current = no galvanic reaction. Always ensure complete separation, not just surface-level protection.

Galvanic corrosion requires metal contact and an electrolyte to occur.صحيح

Both electrical contact and the presence of moisture or an electrolyte are needed for galvanic corrosion to happen.

Simply placing aluminum next to stainless steel with no contact will cause corrosion.خطأ

Corrosion needs direct metal contact and moisture to trigger a galvanic reaction.

Do dielectric coatings prevent galvanic corrosion?

A quick coating seems simple, but does it really stop corrosion between dissimilar metals?

Yes, dielectric coatings prevent galvanic corrosion by creating an insulating layer that blocks electrical flow between aluminum and stainless steel.

Aluminum profile corner angle with insulated design for fastener joints
Aluminum angle profile ideal for isolated stainless bolt connections

Dielectric coatings are non-conductive paints or films. They act like barriers between two different metals. These coatings stop the flow of electrons, which stops the corrosion reaction.

Common types include epoxy, polyurethane, and powder coatings. These are especially useful in marine or outdoor environments where moisture is always present.

Coating Types That Help Prevent Galvanic Corrosion

نوع الطلاء المزايا Lifespan (estimated)
إيبوكسي Tough, chemical resistant 8–10 years
البولي يوريثين UV resistant, flexible 6–8 years
طلاء المسحوق Durable, wide color options 10-15 سنة
Zinc-Rich Primer Sacrificial protection for steel 5-8 سنوات

However, coatings must be continuous. If the coating is scratched or wears off, corrosion can start underneath. Always inspect coated parts regularly.

Dielectric coatings are effective because they stop metal-to-metal contact and current flow.صحيح

They insulate the metals, breaking the electrical path needed for corrosion to occur.

Dielectric coatings work even when applied to only one of the two metals.خطأ

Both metal surfaces must be isolated to fully stop galvanic corrosion. One-sided coating still allows current flow.

How to select fasteners to avoid corrosion?

Fasteners often get ignored, yet they are the most common failure points in mixed-metal designs.

To avoid corrosion, choose fasteners made of compatible metals or isolate them with washers, sleeves, or special coatings.

Industrial aluminum profile designed for structural isolation use
Heavy-duty aluminum designed for insulated mounting with stainless hardware

Using stainless steel bolts on aluminum sounds strong—but it creates a galvanic couple. Over time, the aluminum corrodes around the fastener. That weakens the joint and makes removal hard.

Recommended Fastener Choices for Aluminum Structures

Fastener Type الملاحظات Corrosion Risk
Aluminum fasteners Same metal, no galvanic effect منخفضة جداً
Coated stainless steel With insulation or plating منخفضة
Zinc-coated steel Sacrificial protection, wears over time معتدل
Stainless steel + nylon washers Strong and insulated منخفضة

If you must use stainless steel bolts, combine them with plastic or nylon washers and sleeves. These prevent direct contact. Also consider applying anti-corrosion paste or grease during assembly.

Using stainless steel bolts on aluminum always prevents corrosion due to their durability.خطأ

Stainless bolts can cause aluminum to corrode faster due to galvanic reaction unless isolated.

Aluminum fasteners are the best choice to avoid galvanic corrosion with aluminum parts.صحيح

Same-metal fasteners avoid the galvanic potential difference that causes corrosion.

Is electrical insulation necessary to stop reactions?

It’s not just about the metals—it’s about how electrons move between them. Without a complete circuit, corrosion won’t start.

Yes, electrical insulation is necessary to stop galvanic corrosion because it breaks the circuit between dissimilar metals.

Aluminum trim system with protective coated edge for galvanic resistance
Surface-coated aluminum profile to block electrochemical corrosion

Galvanic corrosion acts like a tiny battery. The metal pair creates voltage. Moisture or another electrolyte connects them. Electrons flow, and aluminum dissolves.

You can block this by interrupting the path:

  1. Use plastic gaskets or sleeves.
  2. Apply full-surface coatings.
  3. Avoid design traps that collect water.
  4. Use isolating brackets or mountings.

Electrical Insulation Checklist

Action Step الغرض
Add rubber or plastic washers Stops direct electrical contact
Paint contact surfaces Insulates metal from each other
Design for drainage Keeps joints dry and electrolyte-free
Use dielectric paste Blocks moisture in fastener threads

Even grounding the system doesn’t help if two dissimilar metals are directly touching. Insulation must be physical and total.

Electrical insulation prevents corrosion by stopping electron flow between metals.صحيح

Without a conductive path, galvanic corrosion cannot occur even if moisture is present.

Grounding the metal structure is enough to stop galvanic corrosion.خطأ

Grounding does not prevent galvanic corrosion; you must break the circuit with insulation.

الخاتمة

Galvanic corrosion between aluminum and stainless steel is preventable. Isolate the metals, coat surfaces, choose the right fasteners, and stop current flow with proper insulation. With the right steps, you can combine these materials safely and effectively.

إيفا

هل ما زلت لا تجد إجابتك؟ يُرجى النقر على الزر أدناه لمزيد من الاستشارات المجانية، إيفا هنا لمساعدتك.
احصل على استشارة مجانية

المنشورات الأخيرة

  • سبتمبر 2، 2025

    متى تزيل فواصل البلاط؟

    يساعد شكل الألومنيوم ذو الفتحة T في الحفاظ على تباعد البلاط بدقة معظم أخطاء التبليط التي رأيتها تحدث بسبب...
    اقرأ المزيد >>>
    مسار ألومنيوم مقذوف على شكل حرف T
  • سبتمبر 2، 2025

    ما هي قناة J-Channel ولماذا تتطابق مع اسمها؟

    مقطع جانبي على شكل حرف J مثالي لتثبيت حواف الجدران الجانبية وإنهاء الحواف الجانبية حافة التنقيط لإغلاق زوايا الجدران الجانبية...
    اقرأ المزيد >>>
    بثق الألومنيوم المقطع J
  • سبتمبر 2، 2025

    كيفية تثبيت حبة زاوية لحواف دريوال قوية؟

    قطع غيار السيارات المخصصة من SinoExtrud تتشقق زوايا الحوائط الجافة بسهولة. بدون تدعيم، حتى الصدمات الخفيفة يمكن أن...
    اقرأ المزيد >>>
arArabic

أرسل لنا رسالة

Google reCaptcha: مفتاح الموقع غير صالح.